Single-layer braided hoses
Product Description
Product introduction
Made of and braided with polyester monofilament and multifilament, it has excellent abrasion resistance, fire resistance and heat dissipation, and is used to provide anti-abrasion protection and noise suppression. The open structure is convenient for the maintenance, upkeep, modification and overhaul of the wrapped objects, suitable for the protection of wire harnesses and piping system of traditional road vehicles and new energy vehicles.
Product characteristics
● Working temperature:: -50°C~150°C
● Flame retardant grade:UL94 HB, FMVSS302
● Halogen free, RoHS compliant
● Standard colors: Black (-0), orange (-1), yellow (-2)
● Laser cutting, smooth incision
Specification and size
|
Product selection TT20 |
Inner diameter (mm) |
Objects that can be wrapped Maximum outside diameter (mm) |
Coincidence rate |
| TT20-5 | 3~6 | 6 | 20%~60% |
| TT20-8 | 3~9 | 9 | 20%~60% |
| TT20-10 | 8~11 | 11 | 20%~60% |
| TT20-13 | 11~14 | 14 | 20%~60% |
| TT20-16 | 14~17 | 17 | 20%~60% |
| TT20-19 | 17~20 | 20 | 20%~60% |
| TT42-25 | 20~26 | 26 | 20%~60% |
| TT42-32 | 27~33 | 33 | 20%~60% |
| TT42-38 | 33~40 | 40 | 20%~60% |

Note:
1、I.D. refers to the round diameter of the sleeving.
2、Special packaging, special color, can be customized
3、Please refer to the Product Specifications Acknowledgement for detailed product parameters
4、Custom polyester or nylon all monofilament self-winding tube products.
| property |
Test methods |
demand |
|
Solubility |
ASTM-D276 | 240℃~265℃ |
|
Thickness change rate |
Take a 300mm long sample and place it in an oven at 120°C for 24h. Take it out from the oven, measure its thickness at 5 points at approximately equal intervals (measuring both before and after the experiment). Rate of change = (Pre-experiment thickness - Post-experiment thickness) / Pre-experiment thickness, taking the absolute value. |
≤10% |
|
Length change rate |
Take a 100mm long sample and place it in an oven at 120°C for 24h. Take it out and measure the length (both before and after the experiment). Rate of change = (Pre-experiment length - Post-experiment length) /Pre-experiment length, taking the absolute value. |
≤10% |
|
Voltage resistance |
Self-rollig tube with metal rod inserted inside and metal foil wrapped outside, 1,000V voltage applied between metal conductors for 1min. |
No breakdown |
|
Abrasion resistance |
Apply 450g of weight on the sample, use 150G gauze abrasion resistant tape (10mm wide conductive portion, maximum 150mm spacing), and run at a speed of 1,500mm/min. When the sample is worn through (conductor portion is in contact with the gauze support pins), record the length of the gauze abrasion resistant tape. |
>1000mm |
|
Flame retardancy |
UL94 FMVSS302 |
HB ≤75mm/min |